DuPont™ Bynel® 4157 Adhesive Resin
Subcategory: Ethylene Vinyl Acetate; Thermoplastic
Material Notes: Bynel® Series 4100 resins are anhydride-modified linear low-density polyethylene (LLDPE) resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyethylene (PE) resins.Applications:Bynel® Series 4100 resins adhere to a variety of materials. They are most often used to adhere to EVOH, polyamide, PE, ionomers, and ethylene copolymers. Bynel® Series 4100 resins can be used in coextrusion processes including: blown filmcast film/sheetblow molding melt and solid phase thermoforming sheet and tubing Bynel® 4157 can also be used in coextrusion coating. LLDPE resins are known for their temperature resistance, clarity and toughness. These physical properties make the Bynel® Series 4100 resins work well in applications such as: boil-in-bag structuresblow molded containers in which drop strength is importantbag-in-box filmsfilm where LLDPE is the heat seal layerInformation provided by DuPont™
| Available Properties |
- Density
- Melt Flow
- Melting Point
- Vicat Softening Point
- Rear Barrel Temperature
- Middle Barrel Temperature
- Front Barrel Temperature
- Adapter Temperature
- Die Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|