DuPont™ Bynel® 42E703 Adhesive Resin
Subcategory: Ethylene Vinyl Acetate; Thermoplastic
Material Notes: Bynel® Series 4200 resins are anhydride-modified low-density polyethylene resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyethylene (PE) resins. Bynel® 42E703 is specifically designed for high bonding performance with EVOH in high-speed coextrusion coating or laminating applications. They can also be used in cast film applications. Physical properties of Bynel® Series 4200 resins are typical of low-density polyethylene resins with similar density and melt index values. Information provided by DuPont™
| Available Properties |
- Density
- Melt Flow
- Melting Point
- Vicat Softening Point
- Rear Barrel Temperature
- Middle Barrel Temperature
- Front Barrel Temperature
- Adapter Temperature
- Die Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|