DuPont™ Elvax® 3135B Ethylene Vinyl Acetate
Subcategory: Ethylene Vinyl Acetate; Thermoplastic
Material Notes: DuPont™ Elvax® 3135B is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins. Additive: antiblock.Applications: This resin is designed to provide a low temperature heat seal to itself or many other materials commonly used in flexible packaging applications. The melt properties of this resin allow it to be processed on blown film equipment over a wide range of film thickness and blow-up ratios. It can also be coextruded with a variety of other polymers. This resin is typically used as low temperature seal layer in coextruded films. Information provided by DuPont™
| Available Properties |
- Density
- Vinyl Acetate Content
- Melt Flow
- Melting Point
- Vicat Softening Point
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|