DuPont™ Nucrel® 30907 Ethylene Acid Copolymer Resin
Subcategory: Ethylene Acrylic Acid; Thermoplastic
Material Notes: Nucrel® 30907 is an ethylene acid copolymer resin available for use in conventional extrusion coating, coextrusion coating, and extrusion laminating equipment designed to process polyethylene resin. This resin may also be used in conventional blown and cast film extrusion and coextrusion equipment.Characteristics: Excellent adhesion to unprimed foil.
Excellent adhesion to coextruded nylon. For superior structure reliability and barrier integrity. Very good hot tack, sealability through contamination, and heat seal strength for strong, reliable heat seals. Lower melt index than Nucrel® 3990 to increase melt strength and to minimize neck-in during extrusion coating operation Applications: Sealants for sachets in both food and non-food applications. Toothpaste tubes as a foil/LDPE tie layer. Other foil-containing pouches and sachets. Medical/pharmaceutical packaging. Cable shield wrap. Information provided by DuPont™
| Available Properties |
- Density
- Melt Flow
- Melting Point
- Vicat Softening Point
- Rear Barrel Temperature
- Middle Barrel Temperature
- Front Barrel Temperature
- Die Temperature
- Casting Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|