DuPont™ Trancend™ Extrusion Coating Sealant
Subcategory: Ethylene Acrylic Acid; Ionomer; Thermoplastic
Material Notes: DuPont™ Trancend™ is an ethylene acrylic acid ionomer, expressly designed for extrusion coating, using a new generation of manufacturing technology. This new technology has allowed DuPont to produce a resin of exceptional value, with unique performance characteristics. The resin is designed to run on standard extrusion coating equipment that is designed to process low density polyethylene and standard ethylene copolymers.Characteristics: Designed as sealant resin capable of unprimed adhesion to aluminum surfaces Heat seal temperatures comparable to DuPont™ Surlyn® 1652 and 9% EAA DuPont™ Nucrel® resins Good hot-tack and seal through contamination performance Cost effective and monolayer and coextruded structures Foil bond durability in the presence of alcohol and oil containing products Information provided by DuPont™
| Available Properties |
- Density
- Melt Flow
- Melting Point
- Vicat Softening Point
- Rear Barrel Temperature
- Middle Barrel Temperature
- Front Barrel Temperature
- Die Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|