DuPont Appeel® LSR 1184 Modified EVA Lidding Sealing Resin
Subcategory: Ethylene Vinyl Acetate; Thermoplastic
Key Words: Ethylene Vinyl Acetate; DuPont Packaging Polymers
Material Notes: Appeel® 1184 is an extrusion coatable resin designed to be a sealing layer for lidding applications. It provides peelable seals over a broad temperature range to a number of container materials including APET, PETG, PP, PS, HIPS, and PVC. Appeel® 1184 is a modified ethylene acrylate polymer available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyethylene resins. Information provided by DuPont Packaging Polymers.
| Available Properties |
- Density
- Viscosity
- Melt Flow
- Seal Strength
- Melting Point
- Vicat Softening Point
- Processing Temperature
- Nozzle Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|