DuPont Bynel® 20E482 Acid-Modified Ethylene Terpolymer Adhesive Resin
Subcategory: EMAAA Terpolymer; Thermoplastic
Close Analogs: This grade is no longer in the DuPont product line
Key Words: DuPont Packaging Polymers
Material Notes: Bynel® Series 2000 resins are acid-modified ethylene terpolymers with medium to high acid comonomer contents. They contain a temperature stable ester that makes them functional in high-temperature coextrusions. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyethylene (PE) resins. Applications: Bynel® Series 2000 resins can be used in a variety of coextrusion coating and laminating applications; for example, laminating metallized films to printed films. They can also be used in thermal lamination processes bonding to a variety of metal, plastic, and paper surfaces. Bynel® 2002, 2022, E403, and 20E482 adhere to a wide variety of materials. They are most often used in coextrusions with PE, EVA, polyamide, and ionomer. They are also useful in adhering to paper, foil, and printed films. Bynel® 2002 and 2022 are designed for low melt temperature coextrusion coating and laminating applications. Bynel® E403 has a melt index suitable for blown or cast film. The primary difference between Bynel® 2002, 2022, and E403 is their rheology. Bynel® 2014 adheres to a wide variety of materials. It is most often used to bond PP films to foil or metallized films. It is also useful in adhering to paper, PE, EVA, PP, and printed films. It has good draw properties and low neck-in, making it especially suited for processes such as coextrusion coating and laminating. It can also be used in film/sheet and tubing. Applications for which Bynel® 2014 is a good resin choice are snack packaging and non-retorted lidding structures in which metal barriers are combined with reverse-printed films. Physical properties of Bynel® Series 2000 resins are typical of ethylene/acrylate copolymer resins with similar density and melt index values. The rheology characteristics of each grade are different, so one may be better suited than the others to a particular extrusion process. Information provided by DuPont Packaging Polymers.
| Available Properties |
- Density
- Viscosity
- Melt Flow
- Melting Point
- Vicat Softening Point
- Processing Temperature
- Nozzle Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|