DuPont Bynel® 50E561 Anhydride-Modified Polypropylene Adhesive Resin
Subcategory: Polypropylene; Thermoplastic
Key Words: PP; DuPont Packaging Polymers
Material Notes: Bynel® Series 5000 resins are anhydride-modified polypropylene. Bynel® 50E561 and 50E571 are based on polypropylene random copolymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polypropylene (PP) resins. Applications: Bynel® Series 5000 resins adhere to a variety of materials. They are most often used to adhere to PP, EVOH, and polyamide. These resins are designed for applications in which EVOH or polyamide is melt coextruded with PP or PP copolymers. Bynel® 50E561 and 50E571 can be used in coextrusion processes including blown film, melt and solid phase thermoforming, and cast film or sheet. Bynel® 50E571 can also be used in extrusion blow molding. Bynel® 50E561 and 50E571 provide outstanding adhesion to EVOH. Physical properties of Bynel® Series 5000 resins are typical of polypropylene resins with similar density and melt index values. The rheology characteristics of each grade are different, so one may be better suited than the others to a particular extrusion process. Information provided by DuPont Packaging Polymers.
| Available Properties |
- Density
- Viscosity
- Melt Flow
- Melting Point
- Vicat Softening Point
- Processing Temperature
- Nozzle Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|