DuPont 20 Series DuPont DPE 20 Specialty Polyethylene Resin
Subcategory: Polyethylene; Thermoplastic
Key Words: DuPont Packaging Polymers
Material Notes: DuPont 20 specialty low density polyethylene resin is characterized by low melt index and intermediate crystallinity. This product, produced via a unique polymerization process, has outstanding flexibility and environmental stress crack resistance. Typical Applications: Extrusion blow molding of medical, pharmaceutical, and personal care containers; Injection and injection blow molding containers and closures; Ophthalmic, inhalant, and nasal solution containers; Low pressure air and water tubing. Features & Benefits: Superior resistance to environmental stress cracking; High flexibility; Good heat stability; Excellent color; Odor free; Excellent chemical resistance; Good mold release performance; Nontoxic. Information provided by DuPont Packaging Polymers.
| Available Properties |
- Density
- Melt Flow
- Hardness, Shore D
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Flexural Modulus
- Izod Impact, Notched
- Izod Impact, Notched, Low Temp
- Melting Point
- Deflection Temperature at 0.46 MPa (66 psi)
- Vicat Softening Point
- Brittleness Temperature
- Refractive Index
- Processing Temperature
- Nozzle Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|