DuPont 20 Series DuPont 2020 Specialty Polyethylene Resin

 

Subcategory: Polyethylene; Thermoplastic; LDPE

Key Words: DuPont Packaging Polymers

Material Notes:
DuPont 2020T and 2020 specialty low density polyethylene resins are products characterized by low melt index and intermediate crystallinity. These products, produced via a unique polymerization process, have a well earned reputation for processability and outstanding flexibility and environmental stress crack resistance. DPE 2020T and 2020 are identical products with DPE 2020T passing a "tube defect" specification that is not required for DPE2020.

Typical Applications: Extruded squeeze tubes for personal care, cosmetic, and pharmaceutical applications; Tube shoulders providing headers for LDPE, HDPE and coextruded squeeze tubes; Low pressure water and air tubing; Rotational molding fittings; Molding of small bottles, caps, seals, etc. for medical, personal care and other applications.

Features & Benefits: Superior resistance to environmental stress cracking; High flexibility; Good heat stability; Excellent color; Odor free; Excellent chemical resistance; Tasteless; Nontoxic.

Each lot of DPE 2020T passes an internal tube imperfection specification.

Information provided by DuPont Packaging Polymers.

Available Properties
  • Density
  • Melt Flow
  • Hardness, Shore D
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break
  • Modulus of Elasticity
  • Flexural Modulus
  • Izod Impact, Notched
  • Izod Impact, Notched, Low Temp
  • Melting Point
  • Deflection Temperature at 0.46 MPa (66 psi)
  • Vicat Softening Point
  • Brittleness Temperature
  • Refractive Index
  • Processing Temperature
  • Nozzle Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。