DuPont Elvax® 3170 Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion, Blown Film
Subcategory: Ethylene Vinyl Acetate; Thermoplastic; Polymer
Key Words: EVA; DuPont Packaging Polymers
Material Notes: 18 wt% Vinyl Acetate. Elvax® 3170 is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins. Additives: Antioxidant.. Applications: Elvax® 3170 is designed to provide a low temperature heat seal to itself or many other materials commonly used in flexible packaging applications. The melt properties of this resin allow it to be processed on blown film equipment over a wide range of film thicknesses and blow-up ratios. It can also be coextruded with a variety of other polymers. Elvax® 3170 is typically used as a low temperature seal layer in coextruded films. Elvax® 3170S and 3170SHB are grades of Elvax® 3170 resin containing FDA approved additives and have been designed to provide films of improved slip and antiblock properties. Information provided by DuPont Packaging Polymers.
| Available Properties |
- Density
- Moisture Vapor Transmission
- Oxygen Transmission
- Viscosity
- Melt Flow
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Secant Modulus, MD
- Secant Modulus, TD
- Impact
- Coefficient of Friction
- Elmendorf Tear Strength, MD
- Elmendorf Tear Strength, TD
- Melting Point
- Vicat Softening Point
- Haze
- Gloss
- Transmission, Visible
- Processing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|