DuPont Elvax® 3176 Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion, Extrusion Coating
Subcategory: Ethylene Vinyl Acetate; Thermoplastic
Key Words: EVA; DuPont Packaging Polymers
Material Notes: 18 wt% Vinyl Acetate. Elvax® 3176 is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins. Additives: Slip, Chill Roll Release, Antioxidant. Information provided by DuPont Packaging Polymers.
| Available Properties |
- Density
- Melt Flow
- Coefficient of Friction
- Melting Point
- Vicat Softening Point
- Processing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|