DuPont Nucrel® 0403 Ethylene-Methacrylic Acid Copolymer Resin for Blown and Cast Film
Subcategory: Ethylene Methyl Acrylate; Thermoplastic; Polymer
Key Words: DuPont Packaging Polymers
Material Notes: 4 wt% Methacrylic Acid. Nucrel® 0403 is an ethylene-methacrylic acid copolymer resin available for use in blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins. Features/Benefits: Adhesion to metallized film. Excellent adhesion to PE. Better hot tack, sealability through contamination and heat seal strength compared to PE. Excellent optical properties. Typical Applications: Tie layer in Surlyn®/TIE/PE type structures. Coextrusion with Nucrel® and PE in film structures. Thermal lamination to metal surfaces. Information provided by DuPont Packaging Polymers.
| Available Properties |
- Density
- Viscosity
- Melt Flow
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Secant Modulus, MD
- Secant Modulus, TD
- Impact
- Graves Tear Strength
- Elmendorf Tear Strength, MD
- Elmendorf Tear Strength, TD
- Dart Drop
- Seal Strength
- Hot Tack Strength
- Melting Point
- Vicat Softening Point
- Haze
- Gloss
- Transmission, Visible
- Processing Temperature
- Nozzle Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|