DuPont Nucrel® 0902HC Ethylene-Methacrylic Acid Copolymer Resin for Blown and Cast Film
Subcategory: Ethylene Methyl Acrylate; Thermoplastic; Polymer
Key Words: DuPont Packaging Polymers
Material Notes: 9 wt% Methacrylic Acid. Nucrel® 0902HC (High-Clarity) is an ethylene-methacrylic acid copolymer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins. Features/Benefits vs. Nucrel® 0403HC: Better adhesion to coextruded nylon for improved structure reliability and barrier integrity. Higher film strength for improved structure reliability and product protection. Lower seal initiation temperature for higher speed packaging. Better hot tack, sealability through contamination, and heat seal strength for stronger, more reliable heat seals. Better film optics for better package appearance and/or better product visibility. Typical Applications: Meat, poultry, seafood, and cheese packaging; Cereal liners; Medical/pharmaceutical packaging; Powdered/granular food and non-food pouches; Carded display/skin packaging films; Edible oil, motor oil, and other liquid product pouches; Snack structures; Coextrusions with nylon or in other film structures as a heat seal or tie layer. Information provided by DuPont Packaging Polymers.
| Available Properties |
- Melt Flow
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Secant Modulus, MD
- Secant Modulus, TD
- Impact
- Elmendorf Tear Strength, MD
- Elmendorf Tear Strength, TD
- Dart Drop
- Hot Tack Strength
- Melting Point
- Vicat Softening Point
- Haze
- Gloss
- Processing Temperature
- Nozzle Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data