DuPont Nucrel® 0903B Ethylene-Methacrylic Acid Copolymer Resin for Blown and Cast Film
Subcategory: Ethylene Methyl Acrylate; Thermoplastic; Polymer
Key Words: DuPont Packaging Polymers
Material Notes: 9 wt% Methacrylic Acid. Nucrel® 0903B is an ethylene-methacrylic acid copolymer resin available for use in blown and cast film extrusion and coextrusion processes designed to process polyethylene resins. Typical Applications: Meat, poultry, seafood, and cheese packaging; Cereal liners; Medical/pharmaceutical packaging; Powdered/granular food and non-food pouches; Carded display/skin packaging films; Edible oil, motor oil, and other liquid product pouches. Features & Benefits: Nucrel® 0903B melt index permits film production at high extrusion rates Use of an antiblock agent helps to prevent film roll blocking. Can be extruded at low temperatures for insurance against off-tastes, off-odors, and taste/odor complaints. Good hot tack, sealability through contamination and heat seal strength provide strong, reliable heat seals. Information provided by DuPont Packaging Polymers.
| Available Properties |
- Melt Flow
- Melting Point
- Vicat Softening Point
- Processing Temperature
- Nozzle Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|