DuPont Nucrel® 0903HC Ethylene-Methacrylic Acid Copolymer Resin for Blown and Cast Film
Subcategory: Ethylene Methyl Acrylate; Thermoplastic; Polymer
Key Words: DuPont Packaging Polymers
Material Notes: 9 wt% Methacrylic Acid. Nucrel® 0903HC (High-Clarity) is an ethylene-methacrylic acid copolymer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins. Features/Benefits vs. Nucrel® 0903: Better film optics provide better package appearance and product visibility. Typical Applications: Meat, poultry, seafood, and cheese packaging; Cereal liners; Medical/pharmaceutical packaging; Powdered/granular food and non-food pouches; Carded display/skin packaging films; Edible oil, motor oil, and other liquid product pouches; Snack structures; Coextrusions with nylon or in other film structures as a heat seal or tie layer. Information provided by DuPont Packaging Polymers.
| Available Properties |
- Melt Flow
- Seal Strength
- Hot Tack Strength
- Melting Point
- Vicat Softening Point
- Processing Temperature
- Nozzle Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|