DuPont Nucrel® 30707 Ethylene-Acrylic Acid Copolymer Resin for Film and Extrusion Coating
Subcategory: Ethylene Acrylic Acid; Thermoplastic; Polymer
Key Words: DuPont Packaging Polymers
Material Notes: 7 wt% Acrylic Acid. Nucrel® 30707 is an ethylene-acrylic acid copolymer resin available for use in blown/cast film and extrusion coating operations. It can be used in both extrusion and coextrusion equipment designed to process polyethylene resins. Features/Benefits: Low seal initiation temperature allows high speed packaging. Very good hot tack, seal through contamination, and heat seal strength provides strong, reliable heat seals. Balanced acid content (7% AA) provides good adhesion to both aluminum and low-density polyethylene (LDPE). In film applications, 7 melt flow index (MFI) allows for very good wetting in thermal lamination processes. In extrusion coating applications, 7 MFI provides better performance in internally deckled dies compared to higher MFI extrusion coating resins. Typical Applications: Cable shield wrap. Sealants for sachets in both food and nonfood applications. Toothpaste tubes, as a foil/LDPE tie layer. Other foil-containing pouches and sachets. Medical/pharmaceutical packaging. Information provided by DuPont Packaging Polymers.
| Available Properties |
- Density
- Melt Flow
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Secant Modulus, MD
- Secant Modulus, TD
- Impact
- Elmendorf Tear Strength, MD
- Elmendorf Tear Strength, TD
- Dart Drop Test
- Seal Strength
- Melting Point
- Vicat Softening Point
- Haze
- Gloss
- Processing Temperature
- Nozzle Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|