DuPont Nucrel® 30707SR Ethylene-Acrylic Acid Copolymer Resin for Film and Extrusion Coating
Subcategory: Ethylene Acrylic Acid; Thermoplastic; Polymer
Close Analogs: This grade is no longer in the DuPont product line
Key Words: DuPont Packaging Polymers
Material Notes: 7 wt% Acrylic Acid. Nucrel® 30707SR is an ethylene-acrylic acid copolymer resin available for use in blown/cast film and extrusion coating operations. It can be used in both extrusion and coextrusion equipment designed to process polyethylene resins. Features/Benefits vs. Nucrel® 30707: Slip additives are added to reduce the coefficient of friction of the film surface to increase operating speeds on packaging machinery. Chill roll release agents are added to enhance extrusion coating speeds by reducing tendency of the hot melt to adhere to the chill roll surface. Typical Applications: Cable shield wrap. Sealants for sachets in both food and nonfood applications. Toothpaste tubes, as a foil/LDPE tie layer. Other foil-containing pouches and sachets. Medical/pharmaceutical packaging. Information provided by DuPont Packaging Polymers.
| Available Properties |
- Density
- Melt Flow
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Secant Modulus, MD
- Secant Modulus, TD
- Impact
- Elmendorf Tear Strength, MD
- Elmendorf Tear Strength, TD
- Dart Drop Test
- Seal Strength
- Hot Tack Strength
- Melting Point
- Vicat Softening Point
- Processing Temperature
- Nozzle Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|