DuPont Nucrel® 31001 Ethylene-Acrylic Acid Copolymer Resin for Blown and Cast Film
Subcategory: Ethylene Acrylic Acid; Thermoplastic; Polymer
Key Words: DuPont Packaging Polymers
Material Notes: 9.5 wt% Acrylic Acid. Nucrel® 31001 is an ethylene-acrylic acid copolymer resin available for use in blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins. Features/Benefits: Excellent adhesion to coextruded nylon for superior structure reliability and barrier integrity. High film strength for excellent structure reliability and product protection. Very good hot tack, sealability through contamination, and heat seal strength for strong, reliable heat seals. Typical Applications: Meat, poultry, seafood, and cheese packaging. Medical/pharmaceutical packaging. Edible oil, motor oil, and other liquid product pouches. Coextrusions with nylon or in other film structures as a heat seal or tie layer. Information provided by DuPont Packaging Polymers.
| Available Properties |
- Density
- Melt Flow
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Secant Modulus, MD
- Secant Modulus, TD
- Impact
- Graves Tear Strength
- Elmendorf Tear Strength, MD
- Elmendorf Tear Strength, TD
- Dart Drop Test
- Seal Strength
- Melting Point
- Vicat Softening Point
- Haze
- Gloss
- Transmission, Visible
- Processing Temperature
- Nozzle Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|