DuPont Selar® PT 4274 Polyester Barrier Resin
Subcategory: Polyester, TP; Thermoplastic; Polymer
Key Words: DuPont Packaging Polymers
Material Notes: Selar® PT 4274 is a toughened homopolymer polyester resin in the high melt viscosity (HMV) series designed for thermoplastic processes. The HMV modification changes the rheology of the melt and provides better processibility in extrusion operations. It can be processed in conventional extruders designed for polyolefins or polyesters. Information provided by DuPont Packaging Polymers.
| Available Properties |
- Density
- Moisture Vapor Transmission
- Oxygen Transmission
- Viscosity
- Film Tensile Strength at Yield, MD
- Film Tensile Strength at Yield, TD
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Secant Modulus, MD
- Secant Modulus, TD
- Impact
- Coefficient of Friction
- Graves Tear Strength
- Elmendorf Tear Strength, MD
- Elmendorf Tear Strength, TD
- Seal Strength
- Melting Point
- Glass Temperature
- Processing Temperature
- Drying Temperature
- Dry Time
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|