DuPont Selar® RB 300 Nylon Blend Barrier Resin
Subcategory: Nylon; Thermoplastic
Close Analogs: This grade is no longer in the DuPont product line
Key Words: Polyamide; DuPont Packaging Polymers
Material Notes: Selar® RB 300 barrier resin is a pellet blend of nylon homolymer and a proprietary adhesive for nylon and polyethylene. Selar® RB 300 is a food grade resin designed for use in blends with polyethylene (HDPE, LDPE, LLDPE) in extrusion blowmolding of articles made with DuPont proprietary Laminar Technology. The DuPont Laminar Technology has also been used for other processes such as sheet extrusion and tube extrusion. Information provided by DuPont Packaging Polymers.
|
|
|
| Property Data |