DuPont Selar® RB 2150 Nylon Barrier Resin
Subcategory: Nylon; Thermoplastic
Close Analogs: This grade is no longer in the DuPont product line
Key Words: Polyamide; DuPont Packaging Polymers
Material Notes: Selar® RB 2150 barrier resin is a nylon copolymer.Selar® RB 2150 has been designed for use in blends with polyethylene (HDPE, LDPE, LLDPE) in extrusion blowmolding of articles made with DuPont proprietary Laminar Technology. The DuPont Laminar Technology has also been used for other processes such as sheet extrusion and tube extrusion. Selar® RB 2150 must be blended with adhesive (Selar® RB A100) prior to use. Information provided by DuPont Packaging Polymers.