DuPont™ Bexloy® AXW602NC010 3% Glass Reinforced, Heat Stabilized Modified Ionomer Resin
Subcategory: Ionomer; Thermoplastic; Polymer
Material Notes: A 3% glass reinforced, heat stabilized modified ionomer resin engineered for injection molded interior automotive applications. Availability: North America Information provided by DuPont.
| Available Properties |
- Density
- Linear Mold Shrinkage
- Melt Flow
- Tensile Strength @ Break
- Elongation at Break
- Flexural Modulus
- Impact Test
- Gardner Impact @ -30°C
- Izod Impact, Notched @ -30°C
- CTE, linear 20°C
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Nozzle Temperature
- Melt Temperature
- Mold Temperature
- Drying Temperature
- Moisture Content
- Back Pressure
- Injection Speed
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|