Dupont™ Fusabond® N MN493D Ethylene Octene Copolymer
Subcategory: Elastomer, TPE; Additive/Filler for Polymer; Thermoplastic
Material Notes: Typical Use: - Nylon 6 toughener
- Nylon 6/6 toughener
Complies to FDA 21CFR 175.105 Availability: North America Information provided by DuPont.
| Available Properties |
- Density
- Melt Flow
- Melting Point
- MAH Graft Level, wt%
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|