Dupont™ Fusabond® E MX110D Linear Low Density Polyethylene
Subcategory: Polypropylene; Additive/Filler for Polymer; Thermoplastic; LLDPE
Material Notes: Typical Use: - Compatibilizer
- Coupling agent for nonhalogen, flame retarded wire and cable compounds containing fillers such as aluminum trihydrate or magnesium hydroxide
- Natural fiber wood-plastic compounds
Availability: North America Information provided by DuPont.
| Available Properties |
- Density
- Melt Flow
- Melting Point
- MAH Graft Level, wt%
|
|
|
|
| Property Data |