Dupont™ Keldax® 1059 Filled Thermoplastic Ethylene Polymer
Subcategory: Thermoplastic; Polymer
Material Notes: A filled thermoplastic ethylene polymer that provides acoustical sound barrier performance in automotive, construction, and industrial applications. Processing Method: Availability: North America Information provided by DuPont.
| Available Properties |
- Density
- Melt Index of Compound
- Hardness, Shore A
- Tensile Strength @ Break
- Elongation at Break
- Flexural Modulus
|
|
|
|
| Property Data |