Dupont™ Elvaloy® 2112 AC Ethylene and 12% Ethyl Acrylate Copolymer

 

Subcategory: Thermoplastic; Polymer

Material Notes:
Elvaloy® 2112 AC is intended for profile and tube extrusion. Its good chemical resistance, low temperature toughness and good flex life make it outstanding for tubing is various applications. The material also is recommended for contour extrusion, as well as for blow molding of toys, gaskets and other parts requiring flexibility, stress cracking resistance and low temperature toughness. Elvaloy® 2112 AC also can be used in film applications where softness and flexibility are needed.

Elvaloy® 2112 AC has a wide processing latitude in molding and extrusion equipment. EEA is very heat stable and does not give corrosive decomposition products during processing, even at the upper limit of the recommended temperature range.

Information provided by DuPont.

Available Properties
  • Density
  • Melt Flow
  • Hardness, Shore A
  • Hardness, Shore D
  • Tensile Strength at Break
  • Elongation at Break
  • Tensile Modulus
  • Melting Point
  • Vicat Softening Point
  • Rear Barrel Temperature
  • Middle Barrel Temperature
  • Front Barrel Temperature
  • Adapter Temperature
  • Die Temperature
  • Melt Temperature
  • EA-Content
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。