Dupont™ Elvaloy® 2615 AC Ethylene and 15% Ethyl Acrylate Copolymer
Subcategory: Thermoplastic; Polymer
Material Notes: Because of its high flexibility and high filler loading capacity, Elvaloy® 2615 AC is particularly suited for injection molded parts in the automotive and furniture industries. It also offers excellent adhesion properties to various substrates and has very good heat stability, making is suitable in extrusion coating and lamination applications. Elvaloy® 2615 AC has a wide processing latitude in molding and extrusion equipment. It has good flow characteristics and lower melting range than low density polyethylene. Information provided by DuPont.
| Available Properties |
- Density
- Melt Flow
- Hardness, Shore A
- Hardness, Shore D
- Tensile Strength at Break
- Elongation at Break
- Tensile Modulus
- Melting Point
- Vicat Softening Point
- Rear Barrel Temperature
- Middle Barrel Temperature
- Front Barrel Temperature
- Adapter Temperature
- Die Temperature
- EA-Content
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|