Dupont™ Elvaloy® 3117 AC Ethylene and 17% Butyl Acrylate Copolymer
Subcategory: Ethylene Butyl Acrylate; Thermoplastic; Polymer
Material Notes: Elvaloy® 3117 AC is intended for coextrusion and compounding. Due to its high melt flow rate, it is used also in extrusion coating. Elvaloy® 3117 AC is soft, flexible and has good adhesion to various polymers. It combines high melting point and good sealing properties. Elvaloy® 3117 AC is easily processed on standard equipment used for low density polyethylene. EBA polymers show excellent thermal stability, which allows higher processing temperatures, if needed. Information provided by DuPont.
| Available Properties |
- Density
- Melt Flow
- Hardness, Shore A
- Hardness, Shore D
- Tensile Strength at Break
- Elongation at Break
- Tensile Modulus
- Melting Point
- Vicat Softening Point
- Rear Barrel Temperature
- Middle Barrel Temperature
- Front Barrel Temperature
- Adapter Temperature
- Die Temperature
- Melt Temperature
- BA-Content
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|