Dupont™ Elvaloy® 3107 AC Ethylene and 7% Butyl Acrylate Copolymer
Subcategory: Ethylene Butyl Acrylate; Thermoplastic; Polymer
Material Notes: Elvaloy® 3107 AC contains antioxidant, slip and antiblock additives. Elvaloy® 3107 AC is developed to give films with good sealing properties, impact strength at lower temperature, and low shrinkage temperature. Elvaloy® 3107 AC is recommended for packaging of deep frozen food, where important properties include heat sealing of the film on high-speed packaging lines. Processing characteristics of Elvaloy® 3107 AC are similar to LDPE and conventional polyethylene extruders are recommended. Information provided by DuPont.
| Available Properties |
- Density
- Thickness
- Melt Flow
- Film Tensile Strength at Yield, MD
- Film Tensile Strength at Yield, TD
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Coefficient of Friction
- Elmendorf Tear Strength, MD
- Elmendorf Tear Strength, TD
- Dart Drop
- Haze
- Gloss
- Rear Barrel Temperature
- Middle Barrel Temperature
- Front Barrel Temperature
- Adapter Temperature
- Die Temperature
- Blow-up Ratio (BUR)
- BA-Content
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|