Dupont™ Elvaloy® 3217 AC Ethylene and 17% Butyl Acrylate Copolymer
Subcategory: Ethylene Butyl Acrylate; Thermoplastic; Polymer
Material Notes: Elvaloy® 3217 AC contains antioxidant, slip and antiblock additives. Elvaloy® 3217 AC has been developed for film applications requiring a combination of softness, toughness and low friction. Typical applications are hygiene films and examination and veterinary gloves. Flexibility and easy sealing make it suitable for colostomy, ileostomy and urinary pouches. Processing characteristics of Elvaloy® 3217 AC are similar to LDPE and conventional polyethylene extruders are recommended. Elvaloy® 3217 AC works very well in both hot bar and high frequency welding units. The low seal temperature ensures short welding cycles and little impact on packed content. The high polarity of EBA gives good performance in high frequency welding. The slip and antiblock content is adapted to production of thin films. For thicker films, mixing with Elvaloy® 3117 is recommended to increase friction. Information provided by DuPont.
| Available Properties |
- Density
- Thickness
- Melt Flow
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Coefficient of Friction
- Rear Barrel Temperature
- Middle Barrel Temperature
- Front Barrel Temperature
- Adapter Temperature
- Die Temperature
- Melt Temperature
- Blow-up Ratio (BUR)
- BA-Content
- Puncture Resistance
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|