DuPont™ Elvax® 40L-03 Ethylene-Vinyl Acetate Copolymer Resin

 

Subcategory: Ethylene Vinyl Acetate; Thermoplastic

Material Notes:
Elvax® 40L-03 is an ethylene-vinyl acetate copolymer that is useful in many wire and cable applications because of its excellent mechanical, thermal, and low-smoke properties. The melt index is appropriate for convenient compounding and extrusion. The melt index is consistent because resin molecular weight distribution is controlled to within a relatively narrow range. The molecular weight is high, so finished products will be relatively resistant to mechanical damage and elevated temperatures.

Compared with other ethylene-vinyl acetate copolymers, Elvax® 40L-03 contains extremely low amounts of gel, or high molecular weight polymer, that can cause undesirable characteristics in finished products

Because Elvax® 40L-03 is somewhat crystalline, it is free flowing and does not mass during handling.

Typical Applications:

  • Jacketing compounds for automotive ignition and low-smoke cables
  • Strippable semiconductive shields for power cables

Features:

  • Narrow molecular weight distribution and low gel properties for consistent and smooth surfaced finished products
  • Stable, long-term cable performance

Information provided by DuPont.

Available Properties
  • Density
  • Vinyl Acetate Content
  • Melt Index of Compound
  • Hardness, Shore A
  • Tensile Strength at Break
  • Elongation at Break
  • Vinyl Acetate Content
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。