DuPont™ Vamac® DP 5.5 phr Peroxide Test Compound
Subcategory: Ethylene Acrylic Acid; Elastomer, TPE; Thermoplastic
Material Notes: Vamac® DP is an ethylene acrylic dipolymer elastomer. Its general performance characteristics are similar to those of the Vamac® terpolymers, including: - Good oil and chemical resistance
- High temperature resistance
- Good compression set resistance
- Good low temperature flexibility
Unlike Vamac® terpolymers, Vamac® DP dipolymer can be processed without a post cure. Form: Bale size is nominally: 560 mm x 370 mm by 165 mm Information provided by DuPont.
| Available Properties |
- Mooney Viscosity
- Hardness, Shore A
- Tensile Strength, Ultimate
- Elongation at Break
- 100% Modulus
- Compression Set
- Armeen® 18D
- HVA® #2 coagent
- Mooney Scorch at 135°C, Minimum Viscosity
- Mooney Scorch at 135°C, t10
- Mooney Scorch at 135°C, t3
- N550 Black
- Naugard® 445 antioxidant
- Stearic Acid
- Vamac® DP
- Vanfre® VAM
- Vulcup® 40LE peroxide
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|