DuPont™ Vamac® DP Activator OC Coagent Test Compound
Subcategory: Ethylene Acrylic Acid; Elastomer, TPE; Thermoplastic
Material Notes: Vamac® DP is an ethylene acrylic dipolymer elastomer. Its general performance characteristics are similar to those of the Vamac® terpolymers, including: - Good oil and chemical resistance
- High temperature resistance
- Good compression set resistance
- Good low temperature flexibility
Unlike Vamac® terpolymers, Vamac® DP dipolymer can be processed without a post cure. Form: Bale size is nominally: 560 mm x 370 mm by 165 mm Information provided by DuPont.
| Available Properties |
- Mooney Viscosity
- Hardness, Shore A
- Tensile Strength, Ultimate
- Elongation at Break
- 100% Modulus
- Tear Strength
- Compression Set
- Glass Temperature
- Activator OC(TAC)
- Armeen® 18D
- Bisoflex T810T
- Change in Volume
- Change in Weight
- Mooney Scorch at 121°C, t5
- Naugard® 445 antioxidant
- Perkadox 14/41
- Stearic Acid
- Sterling SO-N550 black
- Vamac® DP
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|