DuPont™ Vamac® G Sample Compound Vulcanizate Slab Cure (10 minutes at 177°C)
Subcategory: Elastomer, TPE; Ethylene Methyl Acrylate; Thermoplastic
Material Notes: Vulcanizate performance test data can help end-users evaluate the potential fitness of similar compounds for their own applications. Information provided by DuPont.
| Available Properties |
- Hardness, Shore A
- Tensile Strength, Ultimate
- Elongation at Break
- 100% Modulus
- Compression Set
- Brittleness Temperature
- Clash Berg Stiffness Temperature
- Armeen® 18D
- DIAK No. 7(TIAC)
- DOTG Coaccelerator
- Naugard® 445 antioxidant
- SRF Black(N774)
- Stearic Acid
- Vamac® G
- Vanfre® VAM
|
|
|
|