DuPont™ Vamac® GLS Sample Compound
Subcategory: Elastomer, TPE; Ethylene Methyl Acrylate; Thermoplastic
Material Notes: Compounds of Vamac® are formulated and processed by customers to meet their own specific performance requirements. Many of the highest-performing compounds and vulcanizates of Vamac® GLS are thus proprietary, and cannot be published by DuPont. DuPont has independently formulated a wide variety of Vamac® compounds for its own short- and long-term properties testing programs. A typical compound of Vamac® GLS is reviewed below. Information provided by DuPont.
| Available Properties |
- Mooney Viscosity
- Armeen® 18D
- Diak No. 1
- DOTG Coaccelerator
- FEF Black(N550)
- Naugard® 445 antioxidant
- Stearic Acid
- Time for 10 unit Mooney Viscosity Rise
- TP-759
- Vamac® GLS
- Vanfre® VAM
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|