DuPont™ Vamac® GLS Sample Compound Vulcanizate Slab Cure (5 minutes at 177°C)
Subcategory: Elastomer, TPE; Ethylene Methyl Acrylate; Thermoplastic
Material Notes: Test slab is press cured for 5 minutes at 177°C and post cured for 4hrs at 175°C. Vulcanizate performance test data can help end-users evaluate the potential fitness of similar compounds for their own applications. Information provided by DuPont.
| Available Properties |
- Hardness, Shore A
- Tensile Strength, Ultimate
- Elongation at Break
- 100% Modulus
- Tear Strength
- Compression Set
- Glass Temperature
- Armeen® 18D
- Diak No. 1
- DOTG Coaccelerator
- FEF Black(N550)
- Naugard® 445 antioxidant
- Stearic Acid
- TP-760
- Vamac® GLS
- Vanfre® VAM
|
|
|
|