DuPont™ Vamac® HVG Unfilled Gum Ethylene-Acrylic Elastomer
Subcategory: Ethylene Acrylic Acid; Elastomer, TPE; Thermoplastic
Material Notes: Vamac® HVG is an unfilled gum ethylene/acrylic elastomer similar to Vamac® G, but offering higher compound viscosity. The higher viscosity of compounds made with Vamac® HVG results in improved green strength and related processing advantages, such as: - Improved collapse resistance of extrudates
- Enhanced preform dimensional stability
- Improved moldability through elimination of trapped air
Compounds of Vamac® HVG are often selected for applications such as compression molded goods, highly plasticized compounds, and extruded tubing and hose. Vamac® HVG contains a small amount of processing aid. Vamac® HVG is a Vamac® G type polymer with a Mooney Viscosity of 26 compared to 16 for Vamac® G. The two polymers have similar compositions but the Vamac® HVG has a higher molecular weight. They have many common features, including: - Good heat resistance in air
- Good oil and fluid resistance
- Good low temperature properties
- Compounded with similar ingredients
- Cured with same cure package
The big advantage of Vamac® HVG over Vamac® G is that the compounds made from the Vamac® HVG have a higher viscosity. The viscosity of the Vamac® HVG compound can be double that of a Vamac® G compound. This can lead to better processing. Specifically, the potential for a collapsed hose is reduced for an extrusion process and the potential for trapped air in an injection molded compound is reduced. Form: Bale size is nominally: 560 mm x 370 mm by 165 mm Information provided by DuPont.
| Available Properties |
- Density
- Mooney Viscosity
- Collected Volatile Condensable Material
- Color
- Odor
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|