DuPont Elastomers Kalrez® Sahara™ 8085 Gas Deposition Compound
Subcategory: Fluoropolymer, TS; Elastomer, TS; Thermoset
Close Analogs: This former DuPont Dow Elastomers product line is now produced by DuPont Performance Elastomers.
Material Notes: Description: Kalrez® Sahara™ 8085 is a new, specialty compound specifically developed for gas deposition applications, i.e., HDPCVD, PECVD, SACVD, etc. It has been specifically formulated for minimal particle generation in NF3 plasma. Sahara™ 8085 exhibits very low particle generation and low weight loss in oxygen and fluorine plasma, has excellent mechanical properties and is well-suited for both static and dynamic sealing applications (e.g., bonded slit valve doors, bonded gate valves, gas inlets, gas orifice seals, gas feedthrough seals, etc.) A maximum continuous service temperature of 240°C is suggested. Kalrez® Sahara™ 8085 can also withstand short-term excursions up to 275°C. Ultrapure post-cleaning and packaging is standard for parts made from Kalrez® Sahara™ 8085. Information provided by manufacturer.
| Available Properties |
- Hardness, Shore M
- Tensile Strength, Ultimate
- Elongation at Break
- 100% Modulus
- Compression Set, Elevated Temperature
- Maximum Service Temperature, Air
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|