DuPont Elastomers Viton® A-700 Fluoroelastomer (FKM)
Subcategory: Fluoropolymer, TS; Elastomer, TS; Thermoset
Close Analogs: This former DuPont Dow Elastomers product line is now produced by DuPont Performance Elastomers.
Material Notes: Description: Viton® A-700 is an “A-family” gum polymer that has demonstrated easy processing. This gum provides:- Improved compression set resistance
- Good flow for compression molding
- Good mold release
- Less mold fouling
- Improved compression set resistance
- Improved tear properties
Applications: - Compression molding of O-rings, gaskets, and other sealing devices
- Extruded cords, profiles and tubing, or calendered sheets, when a blend of gum polymers are used
- Blending with other polymers for viscosity modification
Information provided by manufacturer.
| Available Properties |
- Density
- Mooney Viscosity
- Chemical Composition
- Color
- Odor
- Physical Form
- Solubility
- Storage Stability
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|