DuPont Elastomers Viton® AL-300 with 30 phr N990 Carbon Black
Subcategory: Fluoropolymer, TS; Elastomer, TS; Thermoset
Close Analogs: This former DuPont Dow Elastomers product line is now produced by DuPont Performance Elastomers.
Material Notes:
Formulation| Viton® AL-300 | 100 | | Carbon Black (N-990) | 30 | | High Activity MgO | 3 | | Calcium Hydroxide | 6 | | Viton® Curative No. 50 | 2.5 | Description: Viton® AL-300 is an “AL-family” gum polymer that demonstrates improved processing when compared to its precursor Viton® B-70N. This gum provides:- Lower viscosity
- Improved mold flow
- Better mold release
- Less mold fouling
- Improved compression set resistance
- Good low temperature characteristics
Applications: - Fuel systems, such as fuel injectors O-rings
- Injection and transfer molding of O-rings, gaskets, and other sealing devices
- Extruded cords, profiles and tubing, or calendered sheets, when a blend of gum polymers are used
- Solution coatings of fabrics and other substrates
Information provided by manufacturer.
| Available Properties |
- Hardness, Shore A
- Tensile Strength, Ultimate
- Elongation at Break
- 100% Modulus
- Tear Strength
- Compression Set, Elevated Temperature
- Brittleness Temperature
- Glass Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|