DuPont Elastomers Viton® B-202/B-600 (75/25) Blend
Subcategory: Fluoropolymer, TS; Elastomer, TS; Thermoset
Close Analogs: This former DuPont Dow Elastomers product line is now produced by DuPont Performance Elastomers.
Material Notes:
Formulation| Viton® B-202 | 75 | | Viton® B-600 | 25 | | MT Black (N-990) | 30 | | Calcium Hydroxide | 6 | | High-Activity MgO | 3 | | Viton® Curative No. 50 | 2.5 | | Viton® Curative No. 20 | 0.5 | Description: Viton® B-202 is a low viscosity, B-type gum polymer that demonstrates improved processing and rheology when compared with existing fluoroelastomers. Viton® B-202 is designed to be cured with either Viton® Curative #30 or Viton® Curative #50. When using Viton® Curative #30, use Viton® Curative #20 in a ratio of about 1.8 Viton® Curative #30 to Viton® Curative #20. When using Viton® Curative #50, use 0.3–0.5 phr of Viton® Curative #20 to ensure a fast cure rate. Note that Viton® Curative #20 can be difficult to mix into low viscosity stocks, such as those based on Viton® B-202, and careful attention needs to be paid to mixing procedures. Compared with other B-family terpolymers, Viton® B-202 provides:- Low viscosity
- Improved processing
- Increased mold flow
- Excellent mold release
Applications: - Transfer and injection molding of complex shapes
- Extrusions (e.g., fuel hose and tubing)
- Solution coatings of fabrics, tanks or chemical containers
Viton® B-202 can be blended with other Viton® types to modify viscosity, enhance processability and/or improve flow. Information provided by manufacturer.
| Available Properties |
- Mooney Viscosity
- Hardness, Shore A
- Tensile Strength, Ultimate
- Elongation at Break
- 100% Modulus
- Compression Set, Elevated Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|