DuPont Elastomers Viton® B-202 with 15 phr N990 Carbon Black

 

Subcategory: Fluoropolymer, TS; Elastomer, TS; Thermoset

Close Analogs: This former DuPont Dow Elastomers product line is now produced by DuPont Performance Elastomers.

Material Notes:
Formulation
Viton® B-20297
Calcium Hydroxide6
MT Black (N-990)15
High-Activity MgO3
Viton® Curative No. 502.5
Viton® Curative No. 200.5

Description: Viton® B-202 is a low viscosity, B-type gum polymer that demonstrates improved processing and rheology when compared with existing fluoroelastomers. Viton® B-202 is designed to be cured with either Viton® Curative #30 or Viton® Curative #50. When using Viton® Curative #30, use Viton® Curative #20 in a ratio of about 1.8 Viton® Curative #30 to Viton® Curative #20. When using Viton® Curative #50, use 0.3–0.5 phr of Viton® Curative #20 to ensure a fast cure rate. Note that Viton® Curative #20 can be difficult to mix into low viscosity stocks, such as those based on Viton® B-202, and careful attention needs to be paid to mixing procedures. Compared with other B-family terpolymers, Viton® B-202 provides:

  • Low viscosity
  • Improved processing
  • Increased mold flow
  • Excellent mold release

Applications:

  • Transfer and injection molding of complex shapes
  • Extrusions (e.g., fuel hose and tubing)
  • Solution coatings of fabrics, tanks or chemical containers

Viton® B-202 can be blended with other Viton® types to modify viscosity, enhance processability and/or improve flow.

Information provided by manufacturer.

Available Properties
  • Mooney Viscosity
  • Hardness, Shore A
  • Tensile Strength, Ultimate
  • Elongation at Break
  • 100% Modulus
  • Compression Set, Elevated Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。