DuPont Elastomers Viton® Extreme™ TBR-605CS with 10 phr N990 Carbon Black and 20 phr Austin Carbon Black
Subcategory: Fluoropolymer, TS; Elastomer, TS; Thermoset
Close Analogs: This former DuPont Dow Elastomers product line is now produced by DuPont Performance Elastomers.
Material Notes:
Formulation| Viton® Extreme™ TBR-605CS | 100 | | High-Activity MgO | 8 | | MT (N990) Carbon Black | 10 | | Austin Carbon Black | 20 | Description: Viton® Extreme™ TBR-605CS (formerly VTR-8802) is a new, base-resistant TFE/propylene polymer, containing a proprietary bisphenol curative. Viton® Extreme™ TBR-605CS utilizes a revolutionary new bisphenol cure site, together with optimized molecular architecture, to provide a polymer that:- Cures quickly, to a high state of cure
- Exhibits excellent mold release and low mold fouling
- Is inherently resistant to attack by basic chemicals
- Provides excellent heat resistance
- Provides superior resistance to hydrocarbon oils compared to other TFE-propylene polymers
- Provides excellent compression set resistance
Information provided by manufacturer.
| Available Properties |
- Hardness, Shore A
- Tensile Strength, Ultimate
- Elongation at Break
- 50% Modulus
- 100% Modulus
- Compression Set, Elevated Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|