Formulation| Viton® 8505 | 100 | | N990 Carbon Black | 30 | | Zinc Oxide | 3 | | Diak™ 7 | 3 | | Varox® DBPH-50 | 3 | Description: VTR-8505 is a new 64% fluorine, peroxide-cured, low-temperature Viton® fluoroelastomer similar to VTR-8500 but with a significantly lower gum polymer viscosity of ~25 (ML at 121°C). VTR-8505 utilizes revolutionary new Advanced Polymer Architecture technology which includes a new peroxide cure site along with an optimized molecular weight distribution designed to deliver a polymer which:- Is ideal for blending with VTR-8500 to reach intermediate viscosity ranges
- Cures exceptionally fast to a high state of cure
- Shows improved mold release/mold fouling properties compared to Viton® GLT and GLT-305
- Shows improved mold flow and less shear sensitivity than 65 Mooney VTR-8500
- Shows excellent physical properties with high elongation, both original and aged
- Shows similar heat, fluids, and low temperature resistance compared to Viton® GLT and GLT-305
- Shows improved water resistance/volume swell in water compared to Viton® GLT and GLT-305
- Shows excellent compression set resistance with either low or no postcure
Information provided by manufacturer.
| Available Properties |
- Mooney Viscosity
- Hardness, Shore A
- Tensile Strength, Ultimate
- Elongation at Break
- Modulus of Elasticity
- 100% Modulus
- Compression Set, Elevated Temperature
- Glass Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|