DuPont Elastomers GFLT-600 Formulation
Subcategory: Fluoropolymer, TS; Elastomer, TS; Thermoset
Close Analogs: This former DuPont Dow Elastomers product line is now produced by DuPont Performance Elastomers.
Material Notes:
Formulation| Viton® GFLT 600 | 100 | | Zinc Oxide | 3 | | N990 Carbon Black | 30 | | Diak™ 7 (TAIC) | 3 | | Luperox® 101-XL peroxide | 3 | Description: VTR-8525 is a new, developmental 66% fluorine peroxide cured polymer that utilizes DuPont Dow's new Advanced Polymer Architecture technology to create an unique new seal offering for fuel systems. VTR-8525, which will become Viton® GBLT-S once it is fully commercial, has the following attributes:- VTR-8525 is a one polymer alternative to GLT and GFLT for fuel seals and fuel injector O-rings
- Better low temperature sealing than GFLT...–40°C and below
- Better fuel/alcohol/methanol resistance than GLT
- Current GFLT and GLT auto specs could be combined into one specification
- VTR-8525 derives additional benefits from new Advanced Polymer Architecture technology
- Physical modulus is low, elongation is high - parts are easier to stretch, more tear resistant in automated assembly equipment
- Cures exceptionally fast to a high state of cure
- Shows improved mold release/mold fouling properties compared to GLT and GFLT
- Shows excellent compression set resistance with little (2 hr at 232°C) or no postcure
It is recommended to use at least 70% load factor in an internal mixer. The recommended process aid for VTR-8525 is 0.5 phr of Armeen® 18D. A two part process aid system of Armeen® 18D with Strucktol WS 280 at 0.8 phr each is optimal if that level of process aid can be tolerated in mold shrinkage. The use of Diak™ #8 is NOT recommended as it causes poor mold release and high compression set. Information provided by manufacturer.
| Available Properties |
- Mooney Viscosity
- Hardness, Shore A
- Tensile Strength, Ultimate
- Elongation at Break
- Modulus of Elasticity
- 100% Modulus
- Compression Set, Elevated Temperature
- Brittleness Temperature
- Glass Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|