DuPont Elastomers VTR 8605/VTR 8600 Blend
Subcategory: Fluoropolymer, TS; Elastomer, TS; Thermoset
Close Analogs: This former DuPont Dow Elastomers product line is now produced by DuPont Performance Elastomers.
Material Notes:
Formulation| VTR 8605 | 50 | | VTR 8600 | 50 | | Zinc Oxide | 3 | | N990 Carbon Black | 30 | | Diak™ 7 (TAIC) | 3 | | Luperox® 101-XL 45 | 2 | Description: VTR-8605 is a new, 70% fluorine, peroxide-cured, Viton® polymer similar to VTR-8600 but with a significantly lower gum polymer viscosity of ~25 (ML at 121°C). VTR-8605 utilizes revolutionary new Advanced Polymer Architecture technology which includes a new peroxide cure site along with an optimized molecular weight distribution designed to deliver a polymer which:- Is ideal for blending with VTR-8600 to reach intermediate viscosity ranges
- Cures exceptionally fast to a high state of cure
- Shows improved mold release/mold fouling properties compared to Viton® GF and GF-300
- Shows improved mold flow and less shear sensitivity than 65 Mooney VTR-8600
- Shows excellent physical properties with high elongation, both original and aged
- Shows similar heat, fluids, and low temperature resistance compared to Viton® GF-300
- Shows improved water resistance/volume swell in water compared to Viton® GF and GF-300
- Shows excellent compression set resistance with either low or no postcure
VTR-8600 is a new, 70% fluorine peroxide cured polymer similar to Viton® GF but utilizes DuPont Dow's new Advanced Polymer Architecture technology which significantly improves processing and curing characteristics. Advanced Polymer Architecture technology in VTR-8600 upgraded the peroxide cure site along with optimizing the molecular architecture to deliver a polymer which: - Cures exceptionally fast to a high state of cure
- Shows improved mold release/mold fouling properties compared to Viton® GF
- Shows improved mold flow, less shear sensitivity, and lower extruder die swell for a ~65 Mooney FKM
- Shows excellent physical properties with high elongation, both original and aged
- Shows similar heat, fluids, and low temperature resistance compared to Viton® GF
- Shows excellent compression set resistance with little (2 hr) or no postcure
When mixing VTR-8600 in an internal mixer it is recommended that at least a 70% load factor be used. Information provided by manufacturer.
| Available Properties |
- Hardness, Shore A
- Tensile Strength, Ultimate
- Elongation at Break
- Modulus of Elasticity
- 100% Modulus
- Compression Set, Elevated Temperature
- Glass Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|