DuPont Elastomers GBL-900 Formulation
Subcategory: Fluoropolymer, TS; Elastomer, TS; Thermoset
Close Analogs: This former DuPont Dow Elastomers product line is now produced by DuPont Performance Elastomers.
Material Notes:
Formulation| Viton® GBL-900 | 100 | | Zinc Oxide | 3 | | N990 Carbon Black | 30 | | Diak™ 7 (TAIC) | 3 | | Luperox® 101-XL peroxide | 3 | Description: VTR-8650 is a new, developmental 68% fluorine peroxide cured polymer similar to Viton® GBL-900 but with significantly improved processing and curing characteristics. VTR-8650 utilizes a revolutionary new Advanced Polymer Architecture technology which includes a new peroxide cure site along with an optimized molecular weight distribution designed to deliver a polymer which:- Cures exceptionally fast to a high state of cure
- Shows improved mold release/mold fouling properties compared to Viton® GBL-900 and 200
- Shows improved mold flow, less shear sensitivity, and lower extruder die swell for a ~65 Mooney FKM
- Shows excellent physical properties with high elongation, both original and aged
- Shows similar heat, fluids, and low temperature resistance compared to Viton® GBL-900 and 200
- Shows improved water resistance/volume swell in water compared to Viton® GBL-900 and 200
- Shows excellent compression set resistance with either low or no postcure
It is recommended if mixing in an internal mixer to use at least a 70% load factor. The recommended process aid for VTR-8650 is 0.5 phr of Armeen® 18D. Information provided by manufacturer.
| Available Properties |
- Mooney Viscosity
- Hardness, Shore A
- Tensile Strength, Ultimate
- Elongation at Break
- Modulus of Elasticity
- 100% Modulus
- Glass Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|