Formulation| Viton® Extreme™ ETP-600S | 100 | | Zinc Oxide | 3 | | N990 Carbon Black | 30 | | Diak™ 7 (TAIC) | 3 | | Luperox® 101XL45 | 3 | Description: Viton® Extreme™ ETP-600S (developmental product VTR-8710) is a new specialty fluoroelastomer, built on DuPont Dow's proprietary Advanced Polymer Architecture (APA) technology, that provides the excellent end-use performance of Viton® Extreme™ ETP-900 with significant improvements in processing and cure characteristics. The APA technology upgrades the peroxide cure site and optimizes the molecular structure to deliver a polymer which:- Cures faster, and to a higher state of cure, than Viton® Extreme™ ETP-900
- Provides excellent mold release and low mold fouling
- Exhibits better mold flow and less shear sensitivity
- Has improved compression set resistance when compared to ETP-900
- Gives the same broad fluid and heat resistance of other Viton® Extreme™ ETP polymers
Viton® Extreme™ ETP-600S takes specialty fluoroelastomer performance to a new level of processing ease combined with the excellent end-use performance. Information provided by manufacturer.
| Available Properties |
- Mooney Viscosity
- Hardness, Shore A
- Tensile Strength, Ultimate
- Elongation at Break
- 50% Modulus
- 100% Modulus
- Compression Set, Elevated Temperature
- Brittleness Temperature
- Glass Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|