DuPont Elastomers Neoprene AG Polychloroprene Rubber
Subcategory: Elastomer, TS; Thermoset
Close Analogs: This former DuPont Dow Elastomers product line is now produced by DuPont Performance Elastomers.
Material Notes: Description: Gel-containing chloroprene polymer designed primarily to provide improved rheology in solvent-based adhesives and mastics. Processing and Performance Features: - Primary use is in contact adhesive and mastics that require thixotropic characteristics. Neoprene AG may be used as the sole polymer or as a modifier for other polymers
- The rheological characteristics of Neoprene AG are superior to those of soluble polymers for producing: spray systems with low cobwebbing and overspray; thixotropic low solids contact adhesives; and nonslumping high solids mastics
- Shear energy is required for proper dispersion of Neoprene AG
Information provided by manufacturer.
| Available Properties |
- Density
- Mooney Viscosity
- Crystallization Rate
- Physical Form and Color
- Polymer Type
- Solubility
- Stability
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|